Your sit:『Products 』
 
 
 『Product list 』
Bottom Brick of Molten Tin Bath   Big Clay Brick Big Kaolin Brick for Bath Zircon Brick 
Aluminum Zirconium Brick Fibrolite Brick for Molten Tin Bath Fibrolite Brick for Feeding Machine
Lightweight Insulation Brick  Hole-sealing Material for Molten Tin Bath Brick Low Air-hole Clay Brick  Zircon Ramming Material Sintered AZS Brick Sintered Mullite Brick

Bottom Brick of Molten Tin Bath


  Bottom Brick of Molten Tin Bath was developed by our Co. in 1986 by unique production process, ramming shaping, filled the gap in China and was widely used on molten tin bath bottom of float glass kilns of 40-odd domestic & foreign float glass production lines with the longest working life in kiln 11 years. The product is of good anti-base and tin corrosion, no scaling, good thermal shock stability, high processing finish, easy installation, etc..

Item
Index
Al2O3(%)
43.5
Fe2O3(%)
1.2
R2O(%)
0.8
Refractoriness(℃)
1750
Load Softening TemperatureT0.6(℃)
1430
Change of Refiring Line(1400℃2h)
+0.0
-0.4
Clear Porosity(%)
18
Volume Density(g/cm3)
2.3
Atmospheric Pressure Strength(MPa)
49
HDiffusion Index(mmH2o)
80
Thermal Stability (1000℃, Water Cooling)
10



  Bottom Brick of Molten Tin Bath of Float Glass Kiln




   Primary Sample of Bottom Brick of Molten Tin Bath Exported from our Co. in Indonesia ARB Float Glass Plant after Cold Overhaul Drainage